Print Friendly Version of this pagePrint Get a PDF version of this webpagePDF

Broad Spectrum Oil-in Water SPF 50 Sunscreen Lotion

This broad spectrum sunscreen lotion is Oxybenzone- and Octocrylene-free and uses SolaStay® S1 to mitigate the photocatalytic and reactive oxygen species generating activity of the oxide and to photostabilize Avobenzone and Octioxate via extremely rapid excited state quenching. The formula was subjected to in vitro analysis and delivered SPF ~60, PFA (PPD) ~27 performance with critical wavelength 382 nm.

Scroll right to view specs →
PhaseINCI Name [INN/USAN] (Other Information)Trade Name% WtFunction
ACaprylic/Capric Triglyceride 3.00Sunscreen Solvent / Emollient
Dicaprylyl Carbonate 3.00Sunscreen Solvent / Emollient
Ethylhexyl Methoxycinnamate [Octinoxate] 7.50UV Filter / Sunscreen Agent
Ethylhexyl MethoxycryleneSolaStay® S1*3.00Photostabilizer
Butyloctyl SalicylateHALLBRITE® BHB*5.00Sunscreen Solvent / Emollient
B4-Methylbenzylidene Camphor [Enzacamene] 4.00UV Filter / Sunscreen Agent
Titanium Dioxide [Titanium Dioxide], Aluminum Hydroxide (60 nm primary particle size) 4.10UV Filter / Sunscreen Agent
CVP/Eicosene Copolymer 1.00Film Former
Glyceryl StearateHALLSTAR® GMS PURE1.60Emulsifier
PEG-100 StearateHALLSTAR® PEG 4400 MS1.60Co-emulsifier
Potassium Cetyl Phosphate, Hydrogenated Palm Glycerides 1.65Emulsifier
DButyl Methoxydibenzoylmethane [Avobenzone] 3.00UV Filter / Sunscreen Agent
EWater (Aqua) (deionized) up to 100Volatile Carrier
Glycerin 3.00Humectant
Disodium EDTA 0.05Chelating Agent
Xanthan Gum (pharma grade) 0.25Thickener (Aqueous)
FPreservative a.n.Preservative
Cyclopentasiloxane 5.00Feel Modification / Enhancement
Aluminum Starch Octenylsuccinate 2.00Deoiling Agent

PREPARATIVE PROCEDURE

1To a secondary vessel add phase A, start mixing and slowly add phase B components individually to phase A with continued mixing.
2Heat phase AB to 85°C and then add phase C ingredients with mixing. Add phase D to phase ABC and mix until phase D is fully dissolved.
3To the main vessel add water and Glycerin of phase E, start mixing, add the Disodium EDTA, then add Xanthan Gum and heat this phase to 80°C.
4When both phases ABCD and EF are homogeneous and at designated temperatures, slowly add phase ABCD to phase EF with mixing.
5Start homogenizing intensively for 3 minutess and start cooling. When the batch is < 50°C, add phase F ingredients one by one with mixing.
6When the batch is uniform add deionized water to correct for evaporative losses. Continue mixing until smooth.

PRODUCT CHARACTERISTICS (25°C)

AppearanceOff-white to pale yellow lotion
Viscosity (Brk, RVDV-II, T-D, 20 rpm, after 24 h at room temperature; mPa∙s)1500 - 3500
pH5.0 - 6.0

*Patented and Patent Pending

The information presented herein is believed to be accurate and reliable, but no warranty or guarantee, expressed or implied, is made regarding the information or the performance of any product. Further, nothing contained herein shall be taken as any inducement or recommendation to use, manufacture or sell that may infringe any patents or any other proprietary rights now or hereafter in existence, nor to imply compliance with any regulatory requirements

The Hallstar Company - 120 South Riverside Plaza Suite 1620 - Chicago, IL 60606-3911 USA

Tel.: 877 427 4255 (International n.: +1 312 385 4494) - Fax: +1 330 929 3616 - E-mail: customerservice@hallstar.com Web Site: hallstar.com